A frame of square tubes looks simpler than it is

Machine frames built from rectangular hollow sections photograph well and are harder to quote. The tube arrives with its own tolerances, the corners need gussets that a welder has to reach, and the faces that carry bearings usually need a pad welded on before anything can be machined.

A tube frame is stiff for its weight and needs less plate than a built-up box. Orders go wrong when the drawing treats the tube as a plate: nominal dimensions, a weld symbol at each corner, and no statement about what the fabricator may assume.

The section standard sets what the frame can hold

Cold formed hollow sections are made to a dimensional standard, and the tolerances in it are wider than most machinery drawings imply. Under EN 10219-2, the outside dimensions of a square or rectangular section are held to plus or minus 1 per cent below 100 mm, 0.8 per cent between 100 and 200 mm, and 0.6 per cent above 200 mm. Wall thickness is plus or minus 10 per cent up to 5 mm and plus or minus 0.5 mm above it. Straightness is 0.15 per cent of length, squareness 90 degrees plus or minus 1 degree, and mass plus or minus 6 per cent on an individual length.

On a 200 x 200 x 8 section, that means the wall can sit between 7.5 and 8.5 mm, and the external corner radius falls between 1.6 and 2.4 times the wall thickness. Weld preparation and fit-up assume one figure. The steel may arrive at the other end of the range.

Two consequences follow. First, any dimension taken from the outside face of a tube carries the section tolerance with it, so a hole pattern positioned from the outside will move relative to a hole pattern positioned from the centre line. Second, a machined face on a tube is only as good as the pad behind it. If a bearing housing is to be bored into an 8 mm wall, the drawing needs a plate thick enough to carry the bore, welded and then machined.

Joint geometry belongs to the designer

A tube frame transfers load through its corners. How that happens is a design decision: a mitred corner, a gusset plate, a coped tee joint or a cast node, each with a different weld volume, inspection burden and tolerance behaviour after welding.

Hollow section joints are not covered by the same simple rules as plate connections. Joint resistance depends on the chord face, the branch angle, the width ratio between branch and chord, and whether the joint is welded on one side or both. Standards for the design of these joints exist, and the calculation is normally done by the party that signs for the structure. A fabricator can build a joint that is drawn. It cannot invent the load path.

This is where enquiries stall. The drawing shows a 45 degree brace meeting a chord with a fillet all round, and nobody has said whether the chord face needs a doubler plate, whether the gap between brace and chord is acceptable, or which weld size applies at the toe. The fabricator prices what it sees, and the difference appears later as a change order or as a frame that moves under load.

Weld access, coping and the angle of the torch

A welder needs to reach the joint at a workable angle. On a tube-to-tube connection that usually means cutting the branch to a profile, coping the corner, or setting the gusset back to leave room for the nozzle.

Three details decide whether the shop can do this cleanly:

  • the cut profile on the branch, and whether it is made on a tube laser or by hand
  • the setback between the branch and the chord face, which controls whether the weld is a gap joint or a close fit
  • the sequence, because a gusset welded into a closed corner cannot be inspected afterwards from the inside

If the drawing does not state these, the shop will choose. The choice is usually the one that is quickest to fit, and it may not be the one the designer assumed when the joint was checked.

Thin walls move, and the drawing has to allow for it

Wall thicknesses between 3 and 8 mm are normal in machinery frames, and they distort more readily than plate of the same thickness because the heat is concentrated near an edge. Angular distortion at a corner pulls the frame out of square, and a frame that is out of square cannot be corrected by machining a face.

The useful levers are known. TWI's guidance on distortion prevention puts the design decisions first: minimise weld metal, avoid over-welding, balance the welding about the joint, and use intermittent welds where the joint allows. A 6 mm fillet specified where a 4 mm fillet carries the load adds metal that pulls the frame and costs time to deposit and inspect.

For a tube frame, the practical additions are a welding sequence agreed before the first pass, a square check after tacking rather than after completion, and a straightening allowance stated in the order. If straightening is not permitted, that has to be written down, because cold or heat correction is normal practice and it changes the residual stress in the frame.

Holes that exist for the galvanizer

A closed tube cannot be dipped in zinc without a way for air to leave and molten metal to enter. The Galvanizers Association's venting guidance is explicit: every sealed section needs venting at each sealed end, holes should sit diagonally opposite one another close to the end plate, and holes in the centre of an end plate or connection trap cleaning fluids and cause bare patches.

The same body's design manual gives the sizing rule used by most galvanizers: hollow sections need at least one vent and one drain hole, each with a diameter equal to 25 per cent of the section's diagonal, or several holes of equivalent area, with 10 mm as a practical minimum. For a 200 x 200 section the diagonal is about 283 mm, so the rule points to roughly 70 mm of opening at each end, split as convenient.

Those holes cannot be left for the galvanizer to add. They are cut in the tube before welding, they change the stiffness of the end, and the drawing has to show their position and size. Where a hole would be unacceptable for structural or sealing reasons, a notch, a cropped corner, or an open end is the alternative, and it needs the same approval.

Bolts through a tube wall

A bolted connection into a hollow section concentrates load on a thin wall. A bolt tightened against an unsupported face will crush the wall before it reaches preload, and a bolt passing through both faces will bend the faces inward.

Three details handle this, and each has a cost:

  • a sleeve or spacer tube between the faces, so the bolt clamps steel against steel
  • a welded insert plate or a thick pad on the face, drilled and tapped
  • a through-bolt with load-spreading washers and a stated preload, accepted by the designer

The drawing should also settle how the hole is sealed, because a tube frame in a wash-down area fills with water and rusts from the inside.

Machined interfaces on a hollow section

Machinery frames usually carry at least one machined interface: a motor pad, a bearing register, a linear rail face. On plate construction, the pad is a thick plate and the machining is straightforward. On tube construction, the pad is a plate welded to the tube face, and the weld pulls the face.

The pad should be thick enough that the bore or register sits in the pad rather than the tube wall, and it should be welded before the frame is machined, so the face is cut after the heat.

Where a rail or a register runs along several metres of tube, straightness becomes the controlling dimension. The section tolerance uses most of a tight straightness budget and welding adds to it. A drawing that asks for 0.2 mm over 3 m on a rail face is asking for a machined surface produced after welding, or for a shimmed rail, and both should be visible in the price.

What the drawing set should contain

For a hollow section frame, the set that prices without argument carries:

  • section size, grade and standard, with the impact requirement stated
  • joint type at every corner, with gusset thickness and setback
  • weld size and length, and the quality class for each joint
  • vent and drain hole position and size, marked before fabrication
  • pad plate thickness at every machined interface, and which faces are machined after welding
  • bolted connection details, including sleeve or insert, and the sealing method
  • straightness and squareness limits, and whether straightening is permitted
  • lifting points, and the weight of the finished frame
  • surface preparation and coating system, with the coating sequence relative to machining

Who owns which decision

The buyer or its engineer owns the joint design, the load path, the section grade and the finish class. Those are the inputs that cannot be recovered later without cutting steel.

The fabricator owns the cut profile, the fit-up, the weld quality to the stated class, the dimensional record and the machining of the interfaces after fabrication. Where the two overlap, the order should say which document wins.

Realjet builds welded frames and structures to customer drawings, with interfaces machined after fabrication, welding to ISO 3834-2 and EN 15085-2 CL1 for rail work, bending from 3,200 to 6,000 mm up to 500 t, and drilling, boring, deburring and sub-assembly inside the same order. Joint design and fatigue assessment sit outside that scope and remain with the party that signs for the structure.

Where to take the question

The contract manufacturing service sets out how made-to-drawing work is scoped, and steel frame fabrication for machinery shows the product side. Hot dip galvanizing and the welded frame RFQ covers the coating decisions that follow from the holes described here, welding distortion control covers the sequence, and weld joint preparation and fit-up covers what the drawing must say about the gap before the first pass.