The joint is chosen before the drawing is finished

Someone places a splice or a base connection during concept design, and every quotation that follows is priced against that choice. The joint decides where the frame is machined, how it travels, what has to be lined up on site, and what the fabricator can prove at dispatch.

Two frames with the same envelope and the same steel grade can differ in price for reasons that have nothing to do with the weld or the bolt. One is welded into a single piece and machined in one set-up. The other is split into bolted modules, machined as separate parts and assembled twice, once in the workshop and once on site.

Both routes work, and most of the trouble comes from drawings that mix them: a bolted joint carrying weld-only tolerance notes, or a welded frame whose hole pattern assumes two separately machined halves.

What a welded frame commits you to

A welded frame is one structure. Stiffness runs through the joint, there is no slip, and a bracket that carries a bearing housing can be welded in place and then bored as part of the assembly. That is why machine bases are usually welded: the machined interface is produced after the heat has done its work, so the bore is square to the frame it actually sits on.

The cost sits in distortion and access. Welding pulls the frame, so the drawing has to leave machining allowance and the shop has to plan for straightening before the faces are cut. Inspection is on the weld, which means a procedure, qualified welders and a quality system behind them rather than a visual check at dispatch. A welded frame also cannot be taken apart later without cutting it.

What a bolted frame commits you to

A bolted frame arrives as plates and members joined with preloaded bolts. It ships in pieces that fit a truck or a container, passes through a doorway, and comes apart for maintenance. Equipment that will be relocated, extended, or moved between plants usually needs that.

What it costs is accuracy at the joint. Both mating faces have to be flat, the hole patterns have to line up, and the joint has to stay tight under the loads the frame sees. Each of those is a manufacturing operation, and each is a place where a low quotation can leave work out without saying so.

Preload, slip and the surface between the plates

Machine frames often specify slip resistant joints, because a frame that shifts a millimetre after commissioning puts the driven machine out of line. EN 1993-1-8 sorts bolted connections into categories: A in bearing, B slip resistant at serviceability, C slip resistant at ultimate, and E preloaded in tension. Categories B and C are the ones that promise no slip, and both work through clamping force rather than bolt shear.

Preload is set at Fp,C = 0.7 fub As. Slip resistance follows from the number of friction surfaces, the slip factor and that preload, divided by a partial factor. Run the numbers on an M20 class 8.8 bolt. The tensile stress area is 245 mm2, so preload is about 137 kN, and with a slip factor of 0.4 the slip resistance lands near 44 kN per friction surface. A bearing type joint would let the same bolt carry far more before it shears, which is why a slip resistant joint needs more bolts for the same load.

The slip factor is not a property of the bolt. The same course notes from CVUT list the friction classes in the standard with factors from 0.2 to 0.5, depending on how the faying surfaces are prepared. Blast cleaning, a zinc silicate coating and a clean mill finish do not land in the same class, and the standard only allows a friction value from testing when the surface is outside the listed classes.

Put the number in the enquiry. A fabricator working from a default may price a category C joint on a surface that only qualifies as category A, and the connection then has to be redesigned or the surface re-prepared after the steel has been cut.

Paint, galvanizing and the friction you paid for

The CVUT notes record French tests in which bolt preload fell by 25 to 45 per cent over two to three months where standard protective paint coatings were used, and they state that such coatings should not be used in slip resistant connections. Special friction paints are accepted where they have been tested.

A specification that asks for a painted frame and a slip resistant joint at the same time creates a conflict. Either the joint is masked and coated with a qualified product, or the joint is designed as bearing type and the frame is allowed to move into bearing under load. Galvanizing raises the same question, because coating thickness changes both the surface and the fit in the holes, and it is applied after the holes are drilled.

Machining: where the two routes separate

On a welded frame, machining comes after welding. The frame is set up on a boring mill or a machining centre, the datum is taken from the structure itself, and the interfaces are cut in one or two set-ups. Feeds and clamping have to work around a part that is large, awkward and already full of residual stress.

On a bolted frame, joint faces are machined as separate parts. Two independently machined faces bolted together stack their errors, and the alignment of the assembly is the sum of both set-ups plus the clearance in the holes. The usual answers are a jig drilled pattern, match drilling during trial assembly, or fitted bolts in reamed holes. Each adds a step, and each has to appear on the drawing if the quotation is to include it.

A drawing can be checked for completeness by asking what the assembly will be measured against. If the answer is the frame's own drawing, the joint faces are being trusted to line up on their own. If the answer is a trial assembly against the mating part, the order carries a step that has to be priced.

What travels, and what has to be lined up again

Transport decides more frames than buyers expect. A frame much over 3 m wide does not travel on a standard flatbed in most countries without a permit, and one longer than a container has to go as break bulk or on deck. Splitting at a joint solves the transport problem, but only if the joint was designed to be re-made: a dowel or a machined register to locate the halves, a bolt pattern that pulls them together evenly, and shim allowance if the foundation is not flat.

Sequence matters as much as geometry. A bolted frame assembled once in the workshop, match marked and dismantled for shipping arrives with a known fit. The same frame shipped as loose plates arrives with an alignment problem that gets solved on site with a drift and a hammer, usually in front of the customer.

Adjustment, maintenance and the second life of the frame

Equipment gets modified. A motor is replaced with a larger frame size, a guard is added, a pump moves to the other side. A bolted frame absorbs that: the module comes off, is re-machined or replaced. A welded frame is cut, which means re-welding, re-machining and re-inspection of the affected area, plus a repaint over a much larger area than the change itself.

Joints can also be checked for preload at intervals, where a weld can only be inspected for cracks. Neither check is free, and the choice belongs to whoever will own the machine for the next fifteen years rather than to whoever signs the first order.

The comparison on the criteria that decide it

Criterion Welded frame Bolted frame
Stiffness through the joint continuous set by preload
Interface accuracy machined after welding two set-ups stacked
Transport width fixed at build splits at the joint
Site work lift and anchor assemble and align
Evidence at dispatch weld and NDT record torque and fit record
Change later cut and re-machine replace a module

What the drawing has to say

  • which joints are welded and which are bolted
  • bolt class and size, and whether the joint is bearing, slip resistant or preloaded
  • hole tolerance and the drilling route: jig, match drill or reamed
  • faying surface preparation, and the coating that will cover it
  • preload method and the record that proves it
  • machining datum, and which faces are machined after fabrication
  • match marking and the trial assembly requirement
  • lifting points, and the weight of each module

Who owns which decision

The buyer or its engineer owns the joint design: loads, slip category, bolt class, coating system and the consequence of a joint that moves. The fabricator owns what comes out of that: hole position, face flatness, weld quality to the stated class, machining to the datum, and the dimensional record that shows the delivered frame matches the approved drawing.

Realjet works to drawings on that basis, with interfaces machined after fabrication, welding to ISO 3834-2 and EN 15085-2 CL1 for rail work, bending from 3,200 to 6,000 mm up to 500 t, and drilling, boring, deburring and sub-assembly inside the same order. Connection design and fatigue assessment are outside that scope. They belong to the party that signs for the structure.

Where to take the question

If the enquiry is for welded frames, base frames, skids or bolted modules made to your drawings, the contract manufacturing service sets out the scope, and custom steel frame fabrication for machinery shows the product side of the same work. Tolerance stack-up in a welded frame covers where the numbers accumulate, machined interfaces covers how to specify them, and repeat welded frame orders covers what carries over to a second order.